- No Items in Cart.
Cronatron® 22 Cast Iron Bare Brazing Rod 3/16"
Cronatron® - 22 Cast Iron Bare Brazing Rod, Gray, 20" Length, 3/16" (5 US Pounds)
Welcome. Register now to see your pricing.
Close
Cronatron® - 22 Cast Iron Bare Brazing Rod, Gray, 20" Length, 3/16" (5 US Pounds)
A selection of brazing alloys for joining cast iron and brazing sheet metal.
Superior Advantages
Solid, dense deposits that can be machined
Free-flowing for thin lapping and butted metal joining
No base metal dilution making tough cast iron repairs possible
True Color Match Cast Iron
Tensile Strength: 53,000 PSIHardness: Rc 18-20Bonding Temperature: 2,300°F (1,260°C)Recommended Flux: F22
Typical Applications
Sheet metal and auto body repairs
Engine heads and blocks
Piping, plumbing and pumps
Gears, sprockets and pulleys
Usage ProcedureUse neutral flame and preheat broad area along braze line. Concentrate flame on rod end and allow weld drops to flow on joint. Continue heating until it wets out and continue process. If a second layer is required, hold torch parallel to the work and apply drop-by-drop. When working with cast iron, avoid localized heating and cover finished braze to retard cooling process.
A selection of brazing alloys for joining cast iron and brazing sheet metal.
Superior Advantages
Solid, dense deposits that can be machined
Free-flowing for thin lapping and butted metal joining
No base metal dilution making tough cast iron repairs possible
True Color Match Cast Iron
Tensile Strength: 53,000 PSIHardness: Rc 18-20Bonding Temperature: 2,300°F (1,260°C)Recommended Flux: F22
Typical Applications
Sheet metal and auto body repairs
Engine heads and blocks
Piping, plumbing and pumps
Gears, sprockets and pulleys
Usage ProcedureUse neutral flame and preheat broad area along braze line. Concentrate flame on rod end and allow weld drops to flow on joint. Continue heating until it wets out and continue process. If a second layer is required, hold torch parallel to the work and apply drop-by-drop. When working with cast iron, avoid localized heating and cover finished braze to retard cooling process.
† May Require Additional Delivery Time to Canada