Certanium® 889 Cast Iron Stick Rod Electrode 3/16"

Certanium® - 889 Cast Iron Stick Rod Electrode, Flux Coated, 180 to 222 HB Hardness, 60 to 100 Amps, DCRP/DCSP/AC Polarity, 3/16" (10 US Pounds) 

Item#: P12009

Price: Log In

Standard Pack: 10   lb

Ship Weight: 10.53

Brand: Certanium®

Usually Ships: Today

Quantity:
Check Stock
Add to List
California Prop 65 WARNING California Proposition 65: WARNING: Cancer -  www.P65Warnings.ca.gov

All-position welding for any type of weldable cast iron repair and cast iron to steel.
Superior Advantages
• High strength welds
• Fully machinable
• Pass-over-pass welding to save time
• All-position welding may eliminate the need to dismantle equipment to perform repairs
For all cast irons – even steel to cast iron
Tensile Strength: Up to 84,000 PSIHardness: 180 – 222 BHNPolarity: AC or DC Straight or Reverse
Typical Applications
• Pump and bearing housings
• Cylinder blocks and heads
• Machine bases
• Manifolds and exhaust systems
Usage Procedure:Remove grease, scale and other impurities from weld area. Bevel cracks or breaks (70° to 90° “V”). CRONACUT™ 1100 is the fastest and easiest method to prepare section for weld repairing. Use a short to medium arc at the lowest possible amperage for best results. Employ weaving technique or stringer beads. Peen to relieve stress. Remove slag between passes. Slow cooling to room temperature recommended.

P12009
Certanium® 889 Cast Iron Stick Rod Electrode 3/16"
Stick
Flux Coated
3/16 "
84,000 PSI
Cast Iron
180-222 BHN
120-170 A
DCRP/DCSP/AC
23271810
Yes

Description

All-position welding for any type of weldable cast iron repair and cast iron to steel.
Superior Advantages
• High strength welds
• Fully machinable
• Pass-over-pass welding to save time
• All-position welding may eliminate the need to dismantle equipment to perform repairs
For all cast irons – even steel to cast iron
Tensile Strength: Up to 84,000 PSIHardness: 180 – 222 BHNPolarity: AC or DC Straight or Reverse
Typical Applications
• Pump and bearing housings
• Cylinder blocks and heads
• Machine bases
• Manifolds and exhaust systems
Usage Procedure:Remove grease, scale and other impurities from weld area. Bevel cracks or breaks (70° to 90° “V”). CRONACUT™ 1100 is the fastest and easiest method to prepare section for weld repairing. Use a short to medium arc at the lowest possible amperage for best results. Employ weaving technique or stringer beads. Peen to relieve stress. Remove slag between passes. Slow cooling to room temperature recommended.

Tech Specs

P12009
Certanium® 889 Cast Iron Stick Rod Electrode 3/16"
Stick
Flux Coated
3/16 "
84,000 PSI
Cast Iron
180-222 BHN
120-170 A
DCRP/DCSP/AC
23271810
Yes

Restrictions

California Prop 65 WARNING California Proposition 65: WARNING: Cancer -  www.P65Warnings.ca.gov
 

Documents:

Back to Top